Re: [MW:17379] PRE HEAT PROCEDURE OF E 7016 -1 ELECTRODE

Dear,
        Do you have Approved consumable Control procedure from your client? then, if you follow the Preheat method as per procedure then no need to worry..check the cause problem,,you will find any way.


On Sat, Apr 13, 2013 at 8:06 AM, jiji lal <jijilalkm@gmail.com> wrote:
SIR,

I'm engaged with welding of API 5LX 80  grade pipeline for regassified LNG transmission . We do  Tie-in method using SMAW+FCAW.
For root pass welding we use E7016-1 electrode after pre heating 250 degree for 2 hr in mother oven and maintain 100 degree in holding oven . during RT interpretation severe hollow bead and porosity observed in root .hence PMC sent almost all joints for repair.now it becomes a serious issue and I think ,the pre heat method was not proper. kindly advice me in this issue.

Mr.Jijilal k .m
qa/qc dept. tecpro ltd.
kochi.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
With Best & Regards

N.Srinivas,
Welding Inspector,
Al Suwaiket Industrial Support Services,
0561198050,0537812787
Al-Khobar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...