many reason
1- how can you check hydro test line check
2-how can painting apply
3-how can check joint during period inspection per year or two year
regards
Mahmoud
qc engineer
Date: Wed, 10 Apr 2013 12:54:55 +0300
Subject: [MW:17330] Pipe joint resting on the beam
From: sumod.sadhupuram@gmail.com
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
1- how can you check hydro test line check
2-how can painting apply
3-how can check joint during period inspection per year or two year
regards
Mahmoud
qc engineer
Date: Wed, 10 Apr 2013 12:54:55 +0300
Subject: [MW:17330] Pipe joint resting on the beam
From: sumod.sadhupuram@gmail.com
To: materials-welding@googlegroups.com
sir,
Please explain the basic reason for not permitting the practice as seen in attached photo.
sumod
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment