Wednesday, April 3, 2013

Re: [MW:17281] HDPE Pipe INSTALLAITION ITP&WPS

Please find the attachment. This I got from Mr. Google.

On Wed, Apr 3, 2013 at 2:53 PM, <mohdfirdaus.abdrahim77@gmail.com> wrote:
Ramesh,

Actually I have the complete procedure for HDPE Pipe underground work. From the details procedure we can create the ITP. HDPE Pipe usually use fusion method either butt fusion or electro fusion. Can you give me jointing method for your work?. Details material use, PN number, size & thickness, product name. I'll try my best to help you.


Mohd Firdaus Abd Rahim
QA/QC

Sent from my iPhone

On 03/04/2013, at 8:52 PG, "manpreet " <manpreetsin88@rediffmail.com> wrote:

Firdaus,

Refrain from commenting if you don't have the correct information, yes there are WPS for HDPE pipe.

Ramesh,

Inbox me a request and I will send you a copy.

Cheers



From: mohdfirdaus.abdrahim77@gmail.com
Sent: Tue, 02 Apr 2013 09:32:54
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: Re: [MW:17268] HDPE Pipe INSTALLAITION ITP&WPS
WPS?. I think there is no need for WPS. 2 type of fusion, electro fusion & butt fusion. It better you google it first before asking. Trust me, you'll find the solution when you google it. I found there too. 

Mohd Firdaus Abd Rahim
QA/QC

Sent from my iPhone

On 02/04/2013, at 11:38 PG, Ramesh <ram2ram_2000@yahoo.com> wrote:

Dear all,
Any one can send HDPE PIPE under ground piping ITP &WPS FORMAT
 Thanks
RAMESH 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


Get your own FREE website and domain with business email solutions, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Best Regard,

Mohd Firdaus Bin Abd Rahim
QA/QC
h/p : +6012-2796361
e-mail : mohdfirdaus.abdrahim77@gmail.com
            seemyskill_77@yahoo.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...