[MW:17353] Quenched annealing of SS 116 Vessel

Dear All,
 
Need your suggestions on PWHT(Quenched annealing) of SS 116 Vessel with following details.

 

1.T.L to T.L=1590mm

2.Totel length=2165mm

3.Shell Dia=1168mm

4.Thickness=10mm

5.Material A240 TP 316L,A312 TP 316,A182 TP 316.

6.Soaking Temperature-1950 ̊F

7.Soaking Time- 105 minutes

8.Rate of Cooling-water Quenching

 

If this Heat Treatment is possible please suggest the good Heat Treatment shop in India.

 

Regards

 

A.K.Pundir

Dy. Manager(Q.A)

MILINDIA LTD.,

W-31, SECTOR-11,

NOIDA - 201 301 (U.P)

09871607731

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...