Friday, February 15, 2013

Re: [MW:16771] P1 MATERIAL TO 2205 MATERIAL

Hi
You can use E2209 or ER2209
Regards
Paul

Sent from my iPad

On 15 Feb 2013, at 5:55 AM, Bala Nechur <bala.Nechur@phoenixindustrial.ca> wrote:

HELLO EXPERTS,

 

i HAVE SOME WELDING 2205 DUPLEX MATERIAL TO P1 GROUP,  FILLET WELD.  PLEASE SUGGEST RECOMMENDED ELECTRODE.

 

BALA

780 204 0239

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...