Friday, February 1, 2013

RE: [MW:16662] Calibration of Flux cored welding machine

Not Possible
 
Current and volt depands upon the load with Input Current or Volt. ( Ammeter and Volt meter must be calibarate for output current or voltage)
 
 


Thank & Best Regards,

 

M Veera SAMY- Bureau Veritas.

Coimbatore

 

 


 

Date: Thu, 31 Jan 2013 07:49:07 -0800
From: spyroxy1@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:16657] Calibration of Flux cored welding machine

Good day all,
 
Please kindly advise on the possibility of calibrating a flux cored welding machine box.. Is it actually possible? if yes, How?
 
Thanks
 
Regards.
 
Ayeni
QAQC Inspector
Nigeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...