dear mohd
we can do the welding GI to SS, provided the GI coating on pipe weld
are to removed by grinding and welding can be carried out with E309
welding electrode.
regards
GSR
On Wed, Jan 16, 2013 at 7:52 AM, <mohdfirdaus.abdrahim77@gmail.com> wrote:
> Dear Expert,
>
> Kindly need your information for stainless pipe weld to G.I pipe. Is it possible to do?. If yes, shall follow which material grouping for G.I pipe?. I need to prepare the WPS for this dissimilar welding. I need to know filler metal to be used etc;.. I hope all of you can guide me. Thank you.
>
> Mohd Firdaus Abd Rahim
> QA/QC
>
> Sent from my iPhone
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:34832] Inquiry about Single Bevel with Back Grinding
Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment