Dear sir,

 

If we go 100 deg  we need to add an temperature -thickness  correction factor for the thickness gauging as per API 570.

 

Regards

 

dinesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of agumarca@yahoo.com
Sent: Monday, January 14, 2013 3:26 PM
To: materials welding
Subject: Re: [MW:16507] Re: Maximum Operating Temp. for UT

 

Hi there are several limit each transducer have limit diferent.
I have ht 400A krautkramer is 800 F.

Best regards

Enviado desde mi BlackBerry de Movistar


From: Raghuram Bathula <raghurambathula@gmail.com>

Sender: materials-welding@googlegroups.com

Date: Sun, 13 Jan 2013 19:35:43 -0800 (PST)

To: <materials-welding@googlegroups.com>

ReplyTo: materials-welding@googlegroups.com

Subject: [MW:16505] Re: Maximum Operating Temp. for UT

 

ES Temp master from .eclipsescientific can be used up to 370 deg c. refer the link below

 

http://www.eclipsescientific.com/Products/Scanning/ESTempMaster/ESTempMaster.pdf

 

 

On Saturday, November 24, 2012 9:10:35 AM UTC+5:30, vicky patil wrote:

Dear Experts,

 

What is the maximum allowable temperature to carry out UT?

 

Regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...