Are you asking about ASME Code qualified welding?
The short answer here CRO or HFO for ASME Code welding is "no". Section IX specifies the WPS/PQR specific testing requirements for overlay welding. If you are looking for ASME compliance, review the corrosion resistant and hard facing overlay requirements there.
The short answer here CRO or HFO for ASME Code welding is "no". Section IX specifies the WPS/PQR specific testing requirements for overlay welding. If you are looking for ASME compliance, review the corrosion resistant and hard facing overlay requirements there.
Craig Franklin Wesson, Jr.
4805 Auburn Drive North M A P
Mobile, AL 36618
cell 336-567-8774
View my LinkedIn profile
gr8fulone@gmail.com
Please consider the environment before printing this email.
<><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><>
This message is confidential, intended only for the named recipient(s), and may contain information that is privileged or exempt from disclosure under applicable law. If you are not the intended recipient(s), you are notified that the dissemination, distribution or copying of this message or any attached files is strictly prohibited. If you receive this message in error, or are not the named recipient(s), please notify the sender at the e-mail address above and discard this e-mail with any attached files immediately.
At the time of transmission, this email and any attachments are believed to be free of any virus or other defect, which might affect any computer system. It is the responsibility of the recipient to check that it is virus-free at the time of receipt. The sender accepts no responsibility or liability for any loss, injury, damage, cost, or expense arising in any way from receipt or use thereof by the recipient.
Thank you.
<><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><>
4805 Auburn Drive North M A P
Mobile, AL 36618
cell 336-567-8774
View my LinkedIn profile
gr8fulone@gmail.com
Please consider the environment before printing this email.
<><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><>
This message is confidential, intended only for the named recipient(s), and may contain information that is privileged or exempt from disclosure under applicable law. If you are not the intended recipient(s), you are notified that the dissemination, distribution or copying of this message or any attached files is strictly prohibited. If you receive this message in error, or are not the named recipient(s), please notify the sender at the e-mail address above and discard this e-mail with any attached files immediately.
At the time of transmission, this email and any attachments are believed to be free of any virus or other defect, which might affect any computer system. It is the responsibility of the recipient to check that it is virus-free at the time of receipt. The sender accepts no responsibility or liability for any loss, injury, damage, cost, or expense arising in any way from receipt or use thereof by the recipient.
Thank you.
<><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><>
On Fri, Jan 11, 2013 at 10:42 PM, Steven Teo <bvsteo@yahoo.com.sg> wrote:
--
Can WPS "V-groove weld details"of welding dis-similar material joints (eg..between CS and SS) also qualify for weld overlay or clad welding ?
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment