Re: [MW:16487] Using of ER70S-6 in place of ER70S-2

Can be used provided if it is available in rod for TIG process.

Generally ER70S2 comes in rod form for TIG welding not in spool form for GMAW process because in GMAW process, Titanium gets oxidided in arc itself and purpose of Ti adding is lost, so it is not at all used in GMAW process.

ER70S6 comes generally in spool forms for GMAW process and if it comes in rod, it can be used in TIG process

Pandithan
Welding Consultant

On Thu, Jan 10, 2013 at 7:48 PM, c sridhar <sridhar305@yahoo.com> wrote:
Mr. Chakraborthy,

You have not given  the  process details. Is it MIG or TIG process.

In general:

For TIG process, we use ER 70S-2 for CS welding. The shielding gas used will be Argon. Radio graphic
quality is assured due to addition of Ti, Zn & Al which removes Oxygen  by forming faster oxides with it
along with Mn.& C. ER 70S-6 is available in spool form ( 15 kg  or so) and not used for TIG process as it
can not provide X-ray quality welds

For MIG process, ER 70S-6 is generally used with  Carbon-DI-oxide as shielding gas. ER 70S-6 has
excessive Mn & Si  (1.85 & 1.15 %  respectively) compared to 1,4 & 0.7 % in ER 70S-2 filler wire,
Additional Mn, & Si will remove oxides form CO2 gas to give good weld quality, but consistency to
provide x-ray quality is a question mark. ER 70S-2 could also be used but, only with Argon gas.

Sridhar.om: Ranendra Chakraborty <ranendrac6@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 10 January 2013 12:13 PM
Subject: [MW:16480] Using of ER70S-6 in place of ER70S-2

Dear Expert,
Please guide whether ER70S-6 can be used in place of ER70S-2. Please give code reference.
 
Regards,
Ranendra
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...