Dear Mr.Hari
My experience is that removing Galv. by flange facing maching ( Remove 1mm thick. of Race)
Thx
S. Pazhanivel
Mechanical Engineer
Target Engineering Construction Company
Mechanical Oil & Gas Division
(Ruwais Refinery Expansion Project-2)
(Ruwais Refinery Expansion Project-2)
Abu Dhabi.
U.A.E
Cell No :+ 971- 50 - 1647754
Cell No :+ 971- 50 - 1647754
Skype Id: spvel13051975
From: Harikrishnan N S <hari.qaqc@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, January 6, 2013 5:55 AM
Subject: [MW:16443] Removing galvanizing from serrated face of flange
Dear Experts
We got some galvanizing deposits on the serrated faces of flanges. Please share some of your experiences in how to remove these deposits without damaging the serrated face. The material is carbon steel.
Thanks and Regards
Harikrishnan N S
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
We got some galvanizing deposits on the serrated faces of flanges. Please share some of your experiences in how to remove these deposits without damaging the serrated face. The material is carbon steel.
Thanks and Regards
Harikrishnan N S
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment