Thursday, January 3, 2013

Re: [MW:16417] P1-P1 qualified WPS for welding API 5L PSL2

Dear Krishna
 
 
Could you provide the following details.
1. Construction code to be followed.
2. Requirement of impact test (temperature and energy).
3. Grade of API 5L pipes to be welded.
4. Whether WPS/PQR for SA 106 Gr.B(P1-P1) Impact tested. If tested -Test temperature.
5. Electrode/filler material used in the WPS/PQR.
 
 
Best Regards,
M.P.N.Muthukumaran
Bureau Veritas - Site@ L&T MFY, Oman.
Mobile: 00 968 94193403
From: krishna <wiqw@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 2 January 2013 4:02 PM
Subject: [MW:16406] P1-P1 qualified WPS for welding API 5L PSL2
Dear Team, We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2 seamless & welded pipes for production and welder qualification. pls share your experiences. thanks, krishna
Catch India as it happens with the Rediff News App. To download it for FREE, click here
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm   The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.    
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...