Wednesday, January 2, 2013

Re: [MW:16408] P1-P1 qualified WPS for welding API 5L PSL2

Dear Krishna,
   surely you can use the same WPS both P group number can use ,if the thickness and diameter should be same.
 
Thanks
M.Riyas

 
On Wed, Jan 2, 2013 at 3:02 PM, krishna <wiqw@rediffmail.com> wrote:
Dear Team,

We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2
seamless & welded pipes for production and welder qualification.

pls share your experiences.

thanks,
krishna

Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...