dear,
You can do PAUT instead of conventional or manual UT.
Regards,
Mohd.
On Jan 3, 1:19 pm, Samun Bhatia <samunbha...@gmail.com> wrote:
> dear all,
>
> we need to carry out UT on anchor flange of pipeline as per drawing.
>
> in the weld neck portion due to the taper profile we are not getting any
> echo while using TR & straight proble.
>
> so in this neck portion what is the method of UT ? do we have to use angle
> probe ?
>
> please reply in detail.
>
> regards,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.
Hello, Please see the response below. Regards. P. Goswami, P. Eng, IWE. From: materials-welding@googlegroups.com <materials-weld...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments: