[MW:16412] RE: 16411] HardnessP-91 Material

Client call typically. You wont find it in B31.1

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Anthony Rudder
Sent: Wednesday, January 02, 2013 11:37 AM
To: materials-welding@googlegroups.com
Subject: [MW:16411] HardnessP-91 Material

 

Sir,

What’s the Max hardness for weld metal and HAZ for P-91 Material per B31.1

 

 

 

 

Thank You,

 

Tony

QA.Manager.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3