[MW:16407] QW407.2 (ASME Sec. IX)

Dear All,

We need little help from you regarding below query for ASME Sec. IX QW-407.2

 

Is it intention of QW-407.2 to have Production Welds Soak Temperature (Vessel Soak temperature) exactly same as that of done in PQR test Coupon?


Thanks in Advance

Tariq Hussain

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...