Re: [MW:15909] Minimum DFT requirement of Pull-off test and Holiday test.

I think the code ISO 4624 (Paints and varnishes : Pull-off test for adhesion). will be helpful to you. below paragraph is the extraction of the same.



You can also refer

  1. ISO 20340:2003, Table 5 – Assessment of test panels – Methods and requirements.
  2. ISO 2409 for cross-cut adhesion tests.

Respectfully,

Nandesh Kumar A


--- On Sun, 11/11/12, Sasikumar.R <sasikumar@punjlloyd.com> wrote:

From: Sasikumar.R <sasikumar@punjlloyd.com>
Subject: [MW:15905] Minimum DFT requirement of Pull-off test and Holiday test.
To: materials-welding@googlegroups.com
Date: Sunday, 11 November, 2012, 1:34 AM

Dear Experts
 
Can I get the information of the Minimum DFT requirement of Pull-off test and Holiday test. In which standard is saying the same.Please advise me.
 
 
Thanks and Regards
Sasikumar.R

This e-mail and any files transmitted with it are for the sole use of the intended recipient(s) and may contain confidential and privileged information. If you are not the intended recipient of this communication, we request you to notify the sender immediately by return email and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email is strictly prohibited.
The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and associated companies (collectively "Punj Lloyd Group") are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any view, opinion or advice expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Punj Lloyd  Group.
Although we have taken all reasonable precautions to ensure that this communication is free from viruses. We do not assume responsibility for any loss or damage arising from the use of this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...