Monday, November 19, 2012

[MW:15970] Re: how many longseam in one shell?

Dear Vicky

 

ASME does not restrict or specify no. of long seam per shell. Just check the client / project specification for such restriction if any specified.

 

Regards

Sudhir Kumar


On Saturday, November 17, 2012 1:58:18 PM UTC+3, vicky patil wrote:
Respected sir,

job heat exchanger id 635mm MOC SS316 make one shell course using 2 plate it means 2 long seam in one shell course, TPIA not accept this then my question is how many longseam in one shell as per asme ?

Regards,,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.