[MW:15877] Enc.: 15825] PWHT -9%Cr-1%Mo/V materials


Conectado pela Motorola


-------- Mensagem original --------
Assunto: Re: 15825] PWHT -9%Cr-1%Mo/V materials
De: Guttemberg <guttemberg.souza@uol.com.br>
Para: pgoswami <pgoswami@quickclic.net>
Cc:

Dear Pradip,

Thank you very much for your aswer!
In fact we have to check the hardness values after PWHT but how many repairs are allowed to do or how many cycles do i have to consider in the WPS qualification as per the metallurgy of these materials?
Greetings,
Guttemberg

Conectado pela Motorola

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...