This is a base metal specification and has no bearing on welded joint porperties; i.e. HAZ or weld metal hardness.
John Henning
________________________________
From: materials-welding@googlegroups.com on behalf of kareem
Sent: Tue 11/6/2012 7:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:15865] Regarding hardness acceptance value for SA-335 P-91 material
Dear experts
As per ASME sec-II SA-335 P-91 material maximum hardness value 250HB. my doubt is how much hardness value accepted (minimum & maximum) for weld metal as well as HAZ.
if have any reference articles please send for me.
Thanks with regards
kareem
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:34832] Inquiry about Single Bevel with Back Grinding
Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment