Dear Experts PQR with Filler wire ER316L Flux SA Cs2 Cr DC; base metal base SA 240 SS316L. Can we use this PQR to weld base metal SA 240 SS304/304L without changing Flux with 308L filler wire! Or re-qualification is required. Thanks & regards Ali Mhaskar, UAE Note: To protect against computer viruses, e-mail programs may prevent sending or receiving certain types of file attachments. Check your e-mail security settings to determine how attachments are handled. | ||
|
Thursday, November 1, 2012
[MW:15827] PQR with Filler wire ER316L Flux SA Cs2 Cr DC can e used on SS304L base metal
Subscribe to:
Post Comments (Atom)
Re: [MW:34913] Filler wire
E71T-1C is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-