Thursday, September 13, 2012

Re: [MW:15304] Repair after PWHT - B 31.1

First thing is you have to do your due dilligence by doing NDT prior to sending for PWHT, so that you wont get caught unaware of the repair before it goes to the oven.
 
Second thing is if there is a repair after PWHT, then you have to cut out the whole weld and redo the weld.
 


 
On Wed, Sep 12, 2012 at 10:17 PM, hemant <hsuthar@chemithon.co.in> wrote:

Dear Jignesh Sir,

As per metallurgy point of view we can done PWHT cycle only one time if we go for second time we have to qualify Repair WPS.  Pls reply me for any suggestion.

 

Thanks,

HHS

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Desai Jignesh (Mumbai - Piping)
Sent: 12 September 2012 09:31
To: materials-welding@googlegroups.com
Subject: RE: [MW:15276] Repair after PWHT - B 31.1

 

I would like to highlight requirement out lined in ASME B 31.3 as below.

 

# Refer Para 341.3.1(a)

 "For P-Nos. 3, 4, and 5 materials, examination shall be performed after completion of any heat treatment"

 

# Refer Note (11) in "NOTES FOR APPENDIX A TABLES " (Pg 147 – 2010 edition)

"For use under this Code, radiography shall be performed after heat treatment"

This note(11) pointing P3, P4, P5A, P5B, P9A & P9B materials only as per table A-1.

 

And of course, Re-PWHT shall be carried out if any repair comes, in case of RT after PWHT.

 

Regds/Jignesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Siva
Sent: 11 September 2012 12:19
To: materials-welding@googlegroups.com
Subject: Re: [MW:15269] Repair after PWHT - B 31.1

 

PWHT shall be done after weld repair. So my understanding is, to find weld repairs, we need to perform NDT before PWHT. I have seen in my experience, normally, NDT will be done prior to and after PWHT also(i.e., twice on that joint).
If NDT done only after PWHT, found any defects, then after weld repair, again should perform PWHT, which might effect mechanical properties.

On Mon, Sep 10, 2012 at 9:10 AM, sevak hiren <hirensevak80@gmail.com> wrote:

Dear Experts,

Piping Code : ASME B 31.1, Power Plant Piping, (P No.5A,11,12,15, 91 etc pipes) & ASME Sectin I

Contractor is doing piping fabrication stages in following manner,

Preheating & Welding of Piping joints then Post heating, then PWHT & then finally RT.

Contractor is arguing, RT is taken after PWHT  to reveal the defects causing due to delayed cracking.

My question

If RT repair is done for particular joint after PWHT then is it compulsory to perform PWHT again for particular joint ? if yes then please mention the clause of code.

Thanks & Regards

Hiren Sevak




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 




--

Regards,
G.Sivalingam., BE.,
Quality Control Inspector - Welding,
SAS Project, Abu Dhabi, UAE.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...