Re: [MW:15285] Use of Group No. 2 Qualified WPS on Group 1 & 2?

Yes, of course.. As group no. is not an essential variable, if impact is not applicable..

Regards,
Josnit

Sent from my iPhone

On Sep 12, 2012, at 9:03, Tariq Hussain <tariqhussain632@gmail.com> wrote:

Dear Expert,

For Vessel (ASME Sec. VIII Div. 1), 
Shell Material = SA 516 Gr. 70N (P. 1 G. 2) Impact Test required per code
Nozzle Pipe Material = SA 333 Gr. 6 (P. 1 G. 1) Impact Test is not Required per code

Can we use a WPS qualified with P.1 G.2 only to weld Nozzle to Shell joint in above mentioned Vessel.

Thanks


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...