RE: [MW:15264] Use of ASME IX WPS for Dissimilar Thickness of More than Range of Groove Weld Thickness Qualified?

See QW-202.4 to determine if the PQR can use, according to the base material.

 

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de Tariq Hussain
Enviado el: Lunes, 10 de Septiembre de 2012 09:46 a.m.
Para: materials-welding@googlegroups.com
Asunto: [MW:15260] Use of ASME IX WPS for Dissimilar Thickness of More than Range of Groove Weld Thickness Qualified?

 

Dear All,

 

Please advise whether A WPS qualified per ASME Sec IX. with PQR Thickness 20mm, can be used for below Joint as shown below, with dissimilar thickness of 92mm and 30mm? As shown in below figure.

Kindly Give Sec, IX clasue reference if possible.

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

 

__________ Información de ESET Smart Security, versión de la base de firmas de virus 7462 (20120910) __________

 

ESET Smart Security ha comprobado este mensaje.

 

http://www.eset.com



__________ Información de ESET Smart Security, versión de la base de firmas de virus 7463 (20120910) __________

ESET Smart Security ha comprobado este mensaje.

http://www.eset.com

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...