Dear Mr Rinshad
Please Mention the Material which u r using for the production of Meshes.
With regards...
MD Sharafudeen
On 9/1/12, rinshad abdul rahman <rinshad043@gmail.com> wrote:
> Dear All,
>
> The photo attached herein showing the wire for screening meshes,we are
> facing the problem of cracking of wire after the crimping (a process which
> is to make meshes from wire).
>
> Can anybody suggest any test method to determine the reason of cracking ?
>
> Is it have any ASTM methods are available ?
>
> The standard for producing the meshes are the following
>
> BS 7372:Part 3 /ISO 4783-3 - Choice of aperture size and wire diameter
> combinations for industrial wire screens and woven wire cloth.
>
> DIN 1SO 14315 - Industrial wire screens technical requirement and testing.
>
> The chemical and mechanical properties are conform to DIN 17223 Part 1
> class A.
>
>
> Thanking you in advance
>
>
> Rinshad
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
Warm Regards...
Mohamed Sharafudeen C.H
Kanpur, Uttar Pradesh
+919758368717,+919847777781
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:34913] Filler wire
E71T-1C is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment