Re: [MW:15189] Impact Test clarification

Yes you can do a supplementary PQR only for Impact satisfying all the Code requirement.
 
Thanks & Regards

J.Gerald Jayakumar
0091-9344954677
From: mubeen mubeen <mubeenaws@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, September 3, 2012 6:33 AM
Subject: [MW:15186] Impact Test clarification

Dear experts, 

Please help out to clear my doubt. 

I have qualified a WPS/PQR with impact -29 deg C, now customer want the WPS/PQR shall be qualified with impact in -46 deg C. Also there is no remaining coupon piece available for impact testing with -46 deg C. 

My question here is, should I weld a coupon and only do impact test as required by customer and attached to PQR will be sort out this issue.? 
or 
Should I REDO a PQR with all mechanical  test which includes Tensile, Hardness, Bend along with impact will sort our this issue.? 


Requesting you to please provide me ASME IX clause reference.


Anticipating for you kind help. 

Thanks & Regards. 
M.K.Mubeen
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...