Re: [MW:15185] PT Rating for unlisted material in ASME B31.3

Look in TEMA. There are tables for different materials.

N. S. Pandit

On Sun, Sep 2, 2012 at 1:03 PM, harsha bhat <harshnb@gmail.com> wrote:
Dear experts,

Following is the details of piping specification:

Pipe: API 5L X60, Flange: A694 F60, Rating: Cl.1500

I need to establish PT rating for A694 F60 (unlisted in ASME B31.3). I checked MSS-SP 44, but it covers up to Cl.900 only.

Can anyone suggest me where to refer pt rating for above said material for Cl.1500?

Thanks in advance.

Regards,
Harsha Bhat.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
N. S. Pandit
alternative e-mail panditns1@rediffmail.com


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...