Hi friends

 

We are using IS 2062 Gr.D E450 (Fe570) for a structural bridge fabrication work in India. The welding process to be used is SMAW and GMAW.

I would like to know the correct SMAW and GMAW consumable for welding IS 2062 Gr.D because very limited information is available about this steel.

ASME Sec IX 2011 addenda has included IS 2062 Gr A,B and C in P1 G1 category but still this steel is an unassigned one till date.

I would be using ER80S-D2 for GMAW and E8018-G for SMAW during PQR, is the selection correct ?

 

Regards

 

Prem Nautiyal

Cell: 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...