Monday, September 3, 2012

[MW:15192] ER 70S-G has A no ?

Dear Experts,

How to explain that ER-70S-G has A No, because A no for GTAW process is an essential variable,
If we refer to ASME sec II C, SFA 5.18 tabel 1 CHEMICAL COMPOSITION REQUIREMENTS FOR SOLID ELECTRODES AND RODS, for ER70S-G is Not Specified..

Thanks for your attention

Best Regards

Deni Rustari

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...