Depending on the service, you might consider E/ER630.

Sent from my BlackBerry® wireless device

From: Roy Liu <standardliu@hotmail.com>
Sender: materials-welding@googlegroups.com
Date: Fri, 6 Jul 2012 15:07:42 +0800
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:14781] what is the proper filler metal for 0Cr19Ni10NbN

hi,all
could any one suggest me that which welding rod is right for the base metal
0Cr19Ni10NbN?
the regular ER347 can not meet the Tensile strength requirement.
 
 
Roy