Thank you very much for your advice.
I have tried to compare the welding profile for both types of electrodes i.e center out and center ok electrodes but both electrodes give the same profile.
Can it be a problem of magnetic arc blow because I felt my electrodes posses some magnetic response?
I have tried to compare the welding profile for both types of electrodes i.e center out and center ok electrodes but both electrodes give the same profile.
Can it be a problem of magnetic arc blow because I felt my electrodes posses some magnetic response?
From: Shadab Ansari <shadabansarialam@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, July 5, 2012 11:54 AM
Subject: Re: [MW:14768] Tapered burning of MMA electrode
Dear Ahmed,
There seems to be the manufacturing problem.
Please check the concentricity of the electrodes. Such problem occurs when the coating and the core rod are not concentric.
There seems to be the manufacturing problem.
Please check the concentricity of the electrodes. Such problem occurs when the coating and the core rod are not concentric.
Warm regards
Shadab ansari
Shadab ansari
On Jul 5, 2012 9:44 AM, "Materials & Welding" <materials-welding@googlegroups.com> wrote:
-- Dear ExpertsI am Facing a problem in SS 308-16 MMA electrode diameter 2.5 mmwhen I start welding It gives tapered burning of electrodewhat can be the possible reasons from welding point of view and electrode manufacturing point of view???How this problem can be solved?Regards,Ahmed--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment