Thursday, July 5, 2012

Re: [MW:14768] Tapered burning of MMA electrode

Dear Ahmed,
There seems to be the manufacturing problem.
Please check the concentricity of the electrodes. Such problem occurs when the coating and the core rod are not concentric.

Warm regards
Shadab ansari

On Jul 5, 2012 9:44 AM, "Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dear Experts
I am Facing a problem in SS 308-16 MMA electrode diameter 2.5 mm 
when I start welding It gives tapered burning of electrode
what can be the possible reasons from welding point of view and electrode manufacturing point of view???
How this problem can be solved?

Regards,
Ahmed

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...