Hi!
To share my experience  is
i) Excentric Flux coating
ii) Improper Flux formulation
 
Regards
 
Hegde P.B.

--- On Thu, 5/7/12, Materials & Welding <materials-welding@googlegroups.com> wrote:

From: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:14767] Tapered burning of MMA electrode
To: materials-welding@googlegroups.com
Date: Thursday, 5 July, 2012, 12:14 PM

Dear Experts
I am Facing a problem in SS 308-16 MMA electrode diameter 2.5 mm 
when I start welding It gives tapered burning of electrode
what can be the possible reasons from welding point of view and electrode manufacturing point of view???
How this problem can be solved?

Regards,
Ahmed
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...