RE: [MW:14759] corrosion under pipe Supports

Dear all,

 

UT CHIME is one of the technique for to measure corrosion under support.

 

 

 

 

Regards

 

Siva

 

Asset Integrity Engineer

 

Operation Assurance

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krish barwar
Sent: Tuesday, July 03, 2012 8:53 PM
To: materials-welding@googlegroups.com
Subject: [MW:14754] corrosion under pipe Supports

 

 

Dear All, 

 

please advice me for inspection  of corrosion under pipe Supports, But Without lifting the pipe from the support. I need to find a quick way of Inspecting the pipes at Each pipe support with some kind of handheld device and NDT to Identify, screen for severity and to measure the Defects Preferably Between the pipe and pipe support.

I tried with guided waves, with bad results. Has anyone successfully tested a system?

 

thanks

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

DISCLAIMER: The information contained in this e-mail may be confidential, proprietary, and/or legally privileged. It is intended only for the person or entity to which it is addressed. If you are not the intended recipient, you are not allowed to distribute, copy, review, retransmit, disseminate or use this e-mail or any part of it in any form whatsoever for any purpose. If you have received this e-mail in error, please immediately notify the sender by return e-mail and delete this e-mail and any attachments immediately. Please be aware that the contents of this e-mail may not be secure and should not be seen as forming a legally binding contract unless otherwise stated.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...