Tuesday, July 3, 2012

Re: [MW:14757] corrosion under pipe Supports


look at the above site. It gives good tips with photographs on pipesupport inspection

arun

On Tue, Jul 3, 2012 at 4:52 PM, krish barwar <krishbarwar007@gmail.com> wrote:


Dear All, 


please advice me for inspection  of corrosion under pipe Supports, But Without lifting the pipe from the support. I need to find a quick way of Inspecting the pipes at Each pipe support with some kind of handheld device and NDT to Identify, screen for severity and to measure the Defects Preferably Between the pipe and pipe support.

I tried with guided waves, with bad results. Has anyone successfully tested a system?


thanks


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arunachalam.A,
Abu Dhabi
0097150-5257122

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...