Re: [MW:14748] Permissible value in decreasing of liquid level in hydrostatic test for aboveground storage tanks

Is tank exposed to the sun?!!

Sent from my iPhone

On Jul 3, 2012, at 11:51 AM, "tugrulhan özdemir" <tugrulhan9@gmail.com> wrote:

Hi everyone
 
 
Is there anyone have an idea about  Permissible value in decreasing of liquid level  in hydrostatic test for aboveground storage tanks.
 
For example  just after filling the tank liquid level was 10610 mm   at 29degre celcious
                           after 5 days the tank liquid level was 10597 mm at 29degre celcious
 
otther infos: New tank , first time for hydrostatic test,  A36 material
 
Thank you
 
 
 
Tugrulhan OZDEMIR
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...