[MW:14838] Verification Of MTC during PQR and WPQ witness

Dear Friends
 
Construction code of a fabricated vessel is ASME Sec. VIII Div.1.
WPS, PQR and WPQ have to be qualified as per ASME Sec. IX.
 
MOC is SA516Gr.70.
 
Now during running the PQR test does the TPI have to verify the base material TC of the PQR test coupons or any stamp transfer has to be checked before welding..
 
Also similarly during Welder qualification do we have to verify the base material TC or any stamp transfer checking for material identification.
 
I think for PQR it is mandatory, but not for WPQ.
 
Please provide code reference and in which clause this is given in AMSE Sec.IX that base material traceability is required before PQR and WPQ test.
 
Regards
 
Prem Nautiyal
Cell: 9769316004
 
 
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point