Monday, July 9, 2012

[MW:14813] Nitrogen in SA 182 Gr. F304L Forgings.

Dear Expers,
 
Good day, As per SA 182 of ASME Sec. IIA, Nitorgen content is mandatory element to be certified in WTC by forgers. Is it acceptable if N2 certified by forger in Product analysis but not certified in Ladle/ heat analysis?
 
Please respond at the earliest.
 
With warm regards,
 
 
C. R. GANDHI
(Manager- Q.A./ Q.C.) 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...