Service Temp. ≤150℃
Acid Condition: PH=2~3
Is ER630 ok?
if no, which Nickel material is ok?
Roy
From: umutcahit@gmail.com
Sent: Saturday, July 07, 2012 2:51 AM
Subject: Re: [MW:14786] what is the proper filler metal for 0Cr19Ni10NbN
Depending on the service, you might consider E/ER630.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Sent from my BlackBerry® wireless device
From: Roy Liu <standardliu@hotmail.com>
Sender: materials-welding@googlegroups.com
Date: Fri, 6 Jul 2012 15:07:42 +0800
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:14781] what is the proper filler metal for 0Cr19Ni10NbN
hi,all
could any one suggest me that which welding rod is right for the base metal
0Cr19Ni10NbN?the regular ER347 can not meet the Tensile strength requirement.
Roy
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment