[MW:14790] Filler Materail required for welding SS 321 to SA 516 gr-70

Dear Experts,

 

I want to weld SA 516 GR-70 plate to SA 182 TP 321.

 

Kindly suggest me the filler material grade used  for welding this material.

 

Thanks & Regards

Ankit Patel
Engineer Quality

 

 

No comments:

Re: [MW:34913] Filler wire