dear lalit,
Lets have following info,
PQR1: GTAW 6 DIA IS FULLY WELEDED WITH GTAW? N WHICH MATERIALS? WHICH
ROD? Impact?
PQR2:PLATE 20 THIK WELDED WITH WHICH PROCESSES?WHICH ELECTRODE ? Is it
with PWHT?impact?
You can combine pqr's in one wps when all other essential variable
same.
Regards,
Mohd.
LALIT VADADORIYA wrote:
> DEAR EXPERTS
>
> WPS FOR GTAW + SMAW PROCESS & SUPPORTING PQR (1) FOR GTAW 6" DIA PIPE
> HAVING 7.11MM THICK AND (2) PLATE HAVING 20 MM THICKNESS IS 2062 GR.B
> MATERIAL.
>
> PIPE THICKNESS 1.5 -20 MM RESTRICTED
>
> WPS QUALIFIED FOR GTAW-3MM AND SMAW 24.11MM THICKNESS, CAN WE ACCEPTED
> THIS ONE OR NOT.
>
> --
> Regards
>
> *Lalit Vadadoriya
> *
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point
Dear Experts. If anyone having presentation of WPS,PQR and WPQ as per ASME SEC.IX in power point then please share . Regards Sanja...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment