Friday, July 6, 2012

[MW:14778] Connecting of ICCP electrodes to the oil pipe



Dear Experts

 

I have a problem during the connecting of Deepwell electrode cable to the oil pipe structure in one of the sites at the south of Iraq. The technical facilities there is limited. Would you please share your technical information with me.

 

Regards,

Dr. Eng. Alaa A. Atiyah

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...