Dear All, 


please advice me for inspection  of corrosion under pipe Supports, But Without lifting the pipe from the support. I need to find a quick way of Inspecting the pipes at Each pipe support with some kind of handheld device and NDT to Identify, screen for severity and to measure the Defects Preferably Between the pipe and pipe support.

I tried with guided waves, with bad results. Has anyone successfully tested a system?


thanks


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...