Diameter is neither an essential, supplementary essential, nor nonessential variable for WPS qualification for common welding processes.   Therefore, any groove weld qualifies groove welds for all diameters for the WPS. 

 

Diameter is an essential for weldor performance qualification for those same processes.  (see QW-353 through QW-357)

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of rafeeqmahadighar rahman
Sent: Monday, July 02, 2012 11:32 AM
To: materials-welding@googlegroups.com
Subject: [MW:14742] Diameter Qualiffication Range for WPS per section IX

 

Dear Experts,

 

Accordance with section IX does the Pipe diameter range is an essential variable for WPS?

for example the PQR coupon has qualified on 8" dia, does it qualify for all or 2 7/8" and above.   

appreciate your valuable input.

 

Warm Regards'

Rafeeq

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...