Monday, July 2, 2012

[MW:14741] Permissible value in decreasing of liquid level in hydrostatic test for aboveground storage tanks

Hi everyone
 
 
Is there anyone have an idea about  Permissible value in decreasing of liquid level  in hydrostatic test for aboveground storage tanks.
 
For example  just after filling the tank liquid level was 10610 mm   at 29degre celcious
                           after 5 days the tank liquid level was 10597 mm at 29degre celcious
 
otther infos: New tank , first time for hydrostatic test,  A36 material
 
Thank you
 
 
 
Tugrulhan OZDEMIR
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...