he must do a 6G test coupon to renew a 6G Welder qualification
--
George Xue (Xue Guoliang)
Suzhou CXGL Mechanical Engineering Co., Ltd.
Tel: +86-512-68639769 Fax: +86-512-68639492
Email: cxueguoliang@gmail.com
Skype: xuegl2001
2012/6/16 raj susi <rjsusi@yahoo.com.sg>:
>
> Dear experts
> Good day.in Asme sec IX for welder qualification-
> in my previous company I have seen that they use production weld followed by Rt to qualify a welder, but now in my new company sometimes they are using production weld and sometimes by a welder qualification coupon.
> So please tell me whether we can do either way or which is best way or in which condition we should follow any of the 2 ways.
> And secondly for renewal of welder qual for 6G position.
> Can we do a test coupon of 1G position and if Rt and other nde passes can he weld 6G position again or he must do a 6G test coupon to renew a 6G Welder qualification.
> Thanks and regards.
> Raj
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
George Xue (Xue Guoliang)
Suzhou CXGL Mechanical Engineering Co., Ltd.
Tel: +86-512-68639769 Fax: +86-512-68639492
Email: cxueguoliang@gmail.com
Skype: xuegl2001
2012/6/16 raj susi <rjsusi@yahoo.com.sg>:
>
> Dear experts
> Good day.in Asme sec IX for welder qualification-
> in my previous company I have seen that they use production weld followed by Rt to qualify a welder, but now in my new company sometimes they are using production weld and sometimes by a welder qualification coupon.
> So please tell me whether we can do either way or which is best way or in which condition we should follow any of the 2 ways.
> And secondly for renewal of welder qual for 6G position.
> Can we do a test coupon of 1G position and if Rt and other nde passes can he weld 6G position again or he must do a 6G test coupon to renew a 6G Welder qualification.
> Thanks and regards.
> Raj
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments