dear , if material is for NACE application , MTC shall recorded the statement as "" Material compliance with MR0175"
 
Product marking is depends  on client requirement , In general alphabet N use as suffix with material grade

Regards


Vinayak Kale
OGSP - QA & I , HC - Upstream
EPC Block , 2nd Floor , Gate No.1
Saki Vihar Rd. Powai Campus
Mumbai - 400072
Ph : + 91 022 6705 3969
(M) - 9987875309
www.larsen toubro.com


-----materials-welding@googlegroups.com wrote: -----
To: materials-welding@googlegroups.com
From: Vino Varghese
Sent by: materials-welding@googlegroups.com
Date: 06/16/2012 08:16PM
Subject: [MW:14566] NACE MR 0175 Requriement / Marking on Product

Dear Experts,
 
Can you please let me know where is the "PRODUCT MARKING" requirement specified in NACE for NACE procured materials.
Eg: ASME piping material refers to ASME A530.
 
Also, whether it is madatory to specify "NACE MR 0175" as product marking?
 
Thanks & Regards
Vino-Doha

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Blog Archive