I assume you can not combine Section IX WPS & API 1104 WPS. (For both the standards , the requirements may be different)

On Fri, Jun 15, 2012 at 11:00 AM, Zeghanu Gigi <zegheanugigi@yahoo.com> wrote:
Dear John,
I saw your experience in welding field on WM site and I would like to ask you something:
I have to combine
1. PQR (Code ASME IX) -2"x5.54mm welded full GTAW 6G pos.-(Base metal ASTM A 106 Gr.B,Filler metal-ER 70 S3).
2. PQR (Code API 1104) -6"x 15.9mm welded full SMAW-6G pos.-(Base metal API 5L X52 ,Filler metal E 6010,Diam.3.2mm for root and cap,E 7010P1/G ,Diam.4mm for Fill.-API 1104.
It is possible?
 
GIGI ZEGHEANU
 
QA/QC /Welding  Dpt.

From: John Henning <jhenning@deltak.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 7 June 2012, 21:19
Subject: [MW:14488] RE: 14478] QW-403.6 OF ASME SEC. IX (MIN. THK. RANGE QUALIFICATION)
Minimum thickness is 6mm.
 
QW-403.6 says ". . . where T is less than 6mm, the minimum thickness qualified is 1/2T . . ." .   Since your thickness is not less than the general rule of T to 2T applies.
 
Note this wording has also given me heart burn.  What I have done is to take a 1/4 inch plate (nominally 6mm) and have the thickness machined to 0.249 inches, this then qualifies for thickness 0.124 to 0.499 inches.  If I need the thickness I will also weld a 1/2 inch thick plate to qualify 1/2 to 1 inch. 
 
Enjoy.
 
John A. Henning
Welding & Materials
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of CHINTUKUMAR GANDHI
Sent: Wednesday, June 06, 2012 5:30 AM
To: materials-welding@googlegroups.com
Subject: [MW:14478] QW-403.6 OF ASME SEC. IX (MIN. THK. RANGE QUALIFICATION)
 
Dear Experts,
 
What shall be the minm. qualified thk. range if PQR is qualified with 6 mm. Nom. thk. with Notch toughness properties. Will it be 3 mm. or 6 mm. as per QW-403.6 of ASME Sec. IX?
 
Further, suppose If I shall qualify this procedure on 5 mm. thk. PQR test coupon (machined from 6 mm. thk.), which thickness shall I have to consider for temperature reduction during subsize test specimen testing? Will it be 5 mm.(actual thk.) or 6 mm. (nom. thk.)?
 
Awaiting your experts' opinion at the earliest.
 
Thanks & regards,
 
 
C. R. GANDHI
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
______________________________________________________________________The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.______________________________________________________________________
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...