ER309 fillerwire is suitable to welding of c.s to ss.
From: Manoj G <manojj.24g@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 14 June 2012 3:52 PM
Subject: [MW:14546] filler used to weld cast iron pipe to SS pipe
Dear all,
Please suggest me the filler to be used to join cast iron pipe with Stainless steel 304 pipe of 5 mm thickness.
Manoj.G