Re: [MW:14545] Distance between two L-Seam

Hi Guru,
 
You can find in ASME VIII Div. I, UW-9 (d).
 
(d) Except when the longitudinal joints are radiographed
4 in. (100 mm) each side of each circumferential welded
intersection, vessels made up of two or more courses shall
have the centers of the welded longitudinal joints of adjacent
courses staggered or separated by a distance of at
least five times the thickness of the thicker plate.
 
Hope it is Ok for U...
 
Cheers,
Sarav,
Korea

On Thu, Jun 14, 2012 at 12:24 PM, Gurunath.Hanamar <guru.h10@gmail.com> wrote:

Dear all,
I know that 100mm is permissble distance between two consecutive longitudinal seams but, can any one confirm minimum distance between two longitudinal seams should be mantained. Kindly mention ASME clause.

Thanks &Regards
Gurunath Hanamar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Blog Archive